JMS_V5_N1_RP3
Joining of Bulk Aluminium Silicon Carbide Metal Matrix Composite
Jeevan Singh Bisht
Apurbba Kumar Sharma
Akshay Dvivedi
Journal on Material Science
2347–615X
5
1
14
22
Al6063, Metal Matrix Composites, Microwave Technology, Mechanical Properties
In this study, an attempt has been made to join MMC (AlSiCp) at interfacial reaction during lap joint. Different specimens of Silicon (Si) particulate reinforced in aluminium matrix were prepared. The various attempts to join MMC have been made using different interfacial joining materials. The obtained strength of lap joint was minimum due to formation of oxides and needs further investigation. Aluminium forms oxide layer within 600 s of application of microwave power of 900 W, during microwave joining. The reaction between two specimens for lap joint resulted in formation of molten aluminum enclosed in aluminium oxide layer. An attempt has been made to break the oxide layer to allow the flow of molten aluminium from one specimen to other.
April - June 2017
Copyright © 2017 i-manager publications. All rights reserved.
i-manager Publications
http://www.imanagerpublications.com/Article.aspx?ArticleId=13482